| Note: Toggle plots by clicking on the legend |
Peak |
T site |
Q-type |
Chemical Shift |
Relative |
Peak Width |
Peak Shape |
Assigment |
(topological) | (ppm) |
Peak Area |
(ppm) |
(x)L (1-x)G |
|
P1 | T2 | Q4(4Al) | -31.73 | 1.000 | 1.51 | 0.245 |
P2 | T1 | Q4(4Al) | -25.58 | 2.000 | 1.60 | 0.245 |
| Authors: | de Onate Martinez, J., McCusker, L.B., Baerlocher, C., Engelhardt, G. | |
| Title: | VPI-5 at 90oC synchrotron powder diffraction study | |
| Reference: | Microporous Mesoporous Mater., 22, 127-134 (1998) |
| Obs. freq. | 162 MHz (Field = 9.4 Tesla) | |
| Pulse sequence | single pulse | |
| MAS frequency | 8-12 kHz | |
| Spectrum | Digitized and processed by Brouwer Lab, Redeemer University | |
| Data processing | Spectrum digitized with WebPlotDigitizer and deconvoluted with Mathematica notebook |
|
| Comment | Peak assignments based on relative peak areas |
| [Al - P - O]-VFI |
| Download digitized spectrum in JCAMP-DX format (This file includes also the data listed on this page) | Download all lines from the above plot in .csv format (This file contains only the plotted data) |