| Material Name: | UCR-20 | ||||
Chemical Formula: |
|(TAEA)16| [Ga32Ge16S96]-RWY TAEA = C6H18N4 = tris(2-aminoethyl)amine = N',N'-bis(2-aminoethyl)ethane-1,2-diamine SMILES: C(CN(CCN)CCN)N Images: stick or |
||||
| Unit Cell: |
cubic |
I -4 3 m (# 217) |
|||
| a' = 20.9352 Å | b' = 20.9352 Å | c' = 20.9352 Å | |||
| α' = 90.000° | β' = 90.000° | γ' = 90.000° | |||
| Framework Density: |
5.2 T/1000 Å3 |
||||
| |
Channels: |
<111> 12 6.9 x 6.9***
| |||||||||||
| Stability: |
Stable when heated in air at 300ºC for 1h (ca 20% weight loss) or at 380ºC in argon |
||||||||||||
| References: |
|||
| Zheng, N., Bu, X., Wang, B. and Feng, P. | |||
| "Microporous and photoluminescent chalcogenide zeolite analogs" | |||
| Science, 298, 2366-2369 (2002) | |||
| |
Name and Code derivation: |
|
|
University of California, Riverside -twenty UCR-20 (twenty) RWY | ||
| Limiting Rings | |
|
|
12-ring viewed along <111> | |